In this research, corrosion resistance of the Cr(III) passivated zincelectrodeposits was evaluated by the neutral salt spray test and electrochemicalmethods. The zinc electrodeposits were passivated in some different Cr(III)passive solutions, resulting in different colors of passive layers. The results of theneutral salt spray test showed that the iridescent Cr(III) passivated sample wasthe most corrosion resistant with 768 hours of testing for reaching 5% white rustarea. These results agreed with those of the electrochemical methods that theiridescent Cr(III) passivated sample was also the most corrosion resistant withthe lowest corrosion current density of 1.59µA/cm2 and the highest passive layerresistance of over 33.89kΩ.cm2. The corrosion resistance of the passivatedsamples decreased in the order of the iridescent passivated samples, the whiteblue passivated samples, the black passivated samples and finally theunpassivated samples.Trong nghiên cứu này, độ bền ăn mòn của các lớp mạ điện kẽm thụ độngCr(III) được đánh giá bằng thử nghiệm phun muối trung tính và các phương phápđiện hóa. Các lớp mạ điện kẽm được thụ động hóa trong một số dung dịch thụđộng Cr(III) khác nhau, cho các lớp thụ động có màu sắc khác nhau. Kết quả thửnghiệm phun muối trung tính cho thấy mẫu thụ động Cr(III) cầu vồng có khảnăng chống ăn mòn cao nhất với diện tích gỉ trắng đạt 5% sau 768 giờ thửnghiệm. Kết quả này phù hợp với kết quả của phương pháp điện hóa mà mẫu thụđộng Cr(III) cầu vồng cũng có khả năng chống ăn mòn cao nhất với mật độ dòngăn mòn thấp nhất là 1,59µA/cm2 và điện trở lớp thụ động cao nhất trên33.89kΩ.cm2. Độ bền ăn mòn của các mẫu thụ động giảm dần theo trật tự sau:mẫu thụ động cầu vồng, mẫu thụ động trắng xanh, mẫu thụ động đen và cuốicùng là mẫu kẽm không thụ động.