Epoxy resin DER 671X75 was modified with fatty acids of soybean oil to improve the toughness of epoxy resin. Fatty acids of soybean oil were separated by saponification with sodium hydroxide solution and acidification with acid sulfuric. Extracted fatty acids and the epoxidized soybean oil resin were characterized by Fourier Transform Infrared Spectrometry (FTIR). The results showed the effects of saponification and acidification conditions on the properties of fatty acids. Epoxy ester resin is synthesized from epoxy resin DER 671X75 and fatty acids of soybean oil with a ratio mass of epoxy resin and fatty acids is 1:2 (wt/wt), reaction temperature of 220 oC, and reaction time with 6 hours for the highest reaction level. Epoxy ester resin was able to form coatings film, and mechanical properties of epoxy polymer coatings film were increasedNhựa epoxy DER 671X75 được biến tính bằng axit béo của dầu đậu nành để cải thiện độ dẻo dai của nhựa epoxy. Các axit béo của dầu đậu nành được tách ra bằng phương pháp xà phòng hóa trong dung dịch natri hydroxit và axit hóa bằng axit sunfuric. Các axit béo được chiết xuất và nhựa epoxy dầu đậu nành được đặc trưng bởi phổ hồng ngoại biến đổi Fourier (FTIR). Kết quả cho thấy ảnh hưởng của điều kiện xà phòng hóa và axit hóa đến tính chất của axit béo. Nhựa epoxy este được tổng hợp từ nhựa epoxy DER 671X75 và axit béo của dầu đậu nành với tỷ lệ nhựa epoxy và axit béo là 1:2 (khối lượng), nhiệt độ phản ứng 220 oC và thời gian phản ứng 6 giờ cho mức độ phản ứng cao nhất. Nhựa epoxy este có khả năng tạo màng và các tính chất cơ học của màng phủ epoxy đã được tăng lên.