In the present paper, nanosized manganese ferrite material is synthesized by the hydrothermal method at temperatures of 190°C in 12 hours. The size and microstructure of MnFe2O4 were analyzed based on X-ray diffraction (XRD), scanning electron microscopy (SEM). The nitrogen adsorption-desorption was used for determination of surface area (Brunauer - Emmett - Teller (BET)) and porosity of the fabricated material. The adsorption behavior of Cr (III) using a new magnetic adsorbent is investigated. The adsorption characteristic and Cr (III) removal efficiency of the adsorbent have been determined by investigating the influence of operating variables such as dosage of manganese ferrite. The maximum Cr (III) sorption capacity was found to be 22.371mg/g and obtained using 0.08g/100mL MnFe2O4 when pH equals 5, a temperature of 25°C, and contact time as 24 hours. The Langmuir, Freundlich and Dubinin - Radushkevichmodels were used to fit the experimental data and these showed good correlations.Trong bài báo này, vật liệu mangan ferit có kích thước nano được tổng hợp bằng phương pháp thủy nhiệt ở nhiệt độ là 190°C trong 12 giờ. Kích thước và cấu trúc vi mô của MnFe2O4 được phân tích dựa trên nhiễu xạ tia X (XRD), kính hiển vi điện tử quét (SEM). Quá trình hấp phụ - giải hấp nitơ được sử dụng để xác định diện tích bề mặt (Brunauer - Emmett - Teller (BET)) và độ xốp của vật liệu tổng hợp được. Sự hấp phụ của Cr (III) lên các hạt nano mangan ferit đã được khảo sát. Đặc tính hấp phụ và hiệu quả loại bỏ Cr (III) của chất hấp phụ đã được xác định bằng cách nghiên cứu ảnh hưởng của liều lượng ferit mangan. Dung lượng hấp thụ Cr (III) tối đa được xác định là 22,37mg/g khi sử dụng 0,08g/100mL MnFe2O4ở pH bằng 5, nhiệt độ 25°C và thời gian tiếp xúc là 24 giờ. Mô hình Langmuir, Freundlich và Dubinin - Radushkevich đã được sử dụng để thử nghiệm các dữ liệu, những mô hình này cho thấy có mối tương quan tốt.