Repair bond strength of resin composite to CAD/CAM glass-ceramic: Influence of cleaning methods, surface treatments, and aging.

 0 Người đánh giá. Xếp hạng trung bình 0

Tác giả: Mariana Silva de Bessa, Boniek Castillo Dutra Borges, Patrícia Dos Santos Calderon, Bruna Oliveira Campos, Isabelle Helena Gurgel de Carvalho, Liliane Cristina Nogueira Marinho, Larissa Mendonça de Miranda, Rodrigo Othávio de Assunção E Souza

Ngôn ngữ: eng

Ký hiệu phân loại:

Thông tin xuất bản: England : Journal of dentistry , 2025

Mô tả vật lý:

Bộ sưu tập: NCBI

ID: 496488

 OBJECTIVE: To evaluate the influence of different cleaning methods, surface treatments, and aging on the repair bond strength to a CAD/CAM glass-ceramic. MATERIALS AND METHODS: Forty-eight lithium disilicate CAD/CAM ceramic blocks were fabricated, sintered, and embedded in acrylic resin. After contamination with human saliva, they were divided according to the factors "Cleaning method" (Control-water/air spray, Air-particle abrasion with Al RESULTS: Significant factors affecting SBS were cleaning method and aging. Surface treatment had an influence but was not statistically significant (p = 0.0591). The IMEP (11.10±2.90 CONCLUSION: Air-particle abrasion with Al CLINICAL SIGNIFICANCE: Lithium disilicate ceramic repair with resin composite is more effective when the ceramic is first decontaminated using a cleaning agent or air-particle abrasion. For conditioning, either MEP or HF followed by silane can be used
  however, MEP presents lower toxicity.