Finding new eco-binders as an alternative to conventional Portland cement in construction activities has recently attracted many researchers worldwide. The feasibility of activating blended fly ash (FA)-ground granulated blast-furnace slag (GGBFS) by commercial Na2SO4 to produce sulfate-activated binder (SAB) was introduced in this study. The SAB samples were prepared with different FA/GGBFS weight ratios of 5/95, 10/90, 15/85, 20/80, and 30/70. Results show that the SAB mixtures exhibited better flowability with more FA inclusion. Before 7 days, the mechanical strength of the SAB samples declined with increasing FA content. However, the samples with 20 and 30% FA exhibited higher strength values at 28 days. Water absorption of the SAB samples was in the ranges of 12.29 - 14.11%. Besides, the inclusion of more FA was beneficial in reducing the drying shrinkage of the SAB samples. The FA/GGBFS ratio of 30/70 was recommended for producing SAB for green and sustainable construction.Việc nghiên cứu chất kết dính mới thân thiện hơn với môi trường để thay thế cho xi măng Poóclăng truyền thống trong các hoạt động xây dựng đã thu hút nhiều nhà nghiên cứu trên thế giới. Tiềm năng của việc hoạt hóa hỗn hợp tro bay (FA)-xỉ lò cao nghiền mịn (GGBFS) bằng Na2SO4 công nghiệp để sản xuất chất kết dính sulfate hoạt hóa (SAB) được giới thiệu trong nghiên cứu này. Các mẫu SAB được chuẩn bị với các tỷ lệ FA/GGBFS (theo khối lượng) là 5/95, 10/90, 15/85, 20/80 và 30/70. Kết quả cho thấy hỗn hợp SAB thể hiện khả năng chảy tốt hơn với hàm lượng FA cao hơn. Trước 7 ngày, cường độ của các mẫu SAB giảm khi hàm lượng FA tăng. Tuy nhiên, cường độ của các mẫu SAB chứa 20 và 30% FA có xu hướng tăng lên ở 28 ngày tuổi. Độ hút nước của các mẫu SAB ở 28 ngày dao động từ 12,29% đến 14,11%. Bên cạnh đó, sử dụng nhiều FA mang lại hiệu quả tích cực trong việc giảm độ co khô của các mẫu SAB. Tỷ lệ FA/GGBFS = 30/70 được khuyến nghị để sản xuất SAB cho mục đích xây dựng bền vững.